1 Ceramic (10 V%) Dispersion Defoaming ARE-250 2 minutes Barium Titanate – 6.02g/cm3 Micron particle, 10 volume %, (Total 120g)
2 Nano Ceramic (70 V%) Dispersion Defoaming ARE-250 3 minutes Aluminum oxide – 0.5µm Nano particle, 3.97g/cm3 50-70 volume %
3 2 part Epoxy Mixing Defoaming ARE-250 20 seconds Epoxy Part A: 3000-6000 poise Part B: 0.3-0.7 poise
4 Carbon Nano Fiber (10V%) Dispersion ARE-250 3 minutes CNF-10 volume % Nano particle, Fiber
5 Carbon Black 2 part silicone (20 wt%) Dispersion Defoaming ARV-310 1 minutes/ ARE-250 8 minutes Nano Carbon Black 20wt% (50V%) Nano particle (Total 120g)
6 Silicone Potting Compounds Mixing Defoaming ARV-310 3 minutes Part A: 4000-8000 poise Part B: 200-700 poise (Total 10g)
7 Precious metal paste Dispersion Defoaming ARV-310 / ARE-250 from 30 sec. to 1 min General silver filled condudctive epoxy / Jar and syringe application Highly dense metal powder
8 Carbon NanoTube (1-2 wt%) Dispersion ARV-310 6 min CNT – 1-2 wt% Nano particle tube
9 Zinc Oxide(10 V%) Dispersion Defoaming ARE-250 6 min ZnO 10 volume % petroleum Jelly 0.85, Zinc Oxide 5.76
10 LCD ODF sealant (10V%) Dispersion Deforming ARV-5000 TWIN Au Ball 10 volume % sealant 400,000cP, Au ball 3µ
11 Printing Ink Degas ARV-5000 Solvent Ink 450g
12 Viscous Epoxy Defoaming ARE-250250AD-EFD-3×6 Epoxy 828 2.5cc in EFD 3cc Syringe
13 Alumina Dispersion Defoaming ARV-5000 Aluminum oxide – 20 volume % Silicone 3000cP
14 LED Phosphor Dispersion Defoaming ARV-310+ Syringe Loader Phosphor 10 wt% Slicone 10,000cP 20g
15 Viscous Epoxy Defoaming ARV-310 + Syringe Loader Various Epoxy sample
16 Talc DispersionDefoaming ARE-250 Silicone 60g – 30wt% Silicone 10,000cP
17 CNF (1%wt) Dispersion Defoaming ARV-310 6min CNF 1%wt
18 Suspension Particle Reduction ARE-250 3min Phenytoin as API